Lead alloys are attractive candidates as coolants for future generation nuclear reactors (fast reactors). Unfortunately, they easily corrode structural steels of reactors. To mitigate this phenomenon, surface protective coatings may be applied. In this study, T91 steel (Cr9Mo1) samples were coated with aluminum oxide coatings (Al-O) deposited by radio frequency magnetron sputtering. The alumina coatings were characterized using scanning electron microscopy–energy dispersive spectroscopy, x-ray diffraction, and tribological techniques. A corrosion test of coated steel samples was performed in stagnant lead at 550 °C for 1200 h and none of the samples revealed corrosion signs.

1.
L.
Cinotti
,
C. F.
Smith
,
H.
Sekimoto
,
L.
Mansani
,
M.
Reale
, and
J. J.
Sienicki
,
J. Nucl. Mater.
415
,
245
(
2011
).
2.
Nuclear Energy Agency
.
Handbook on Lead-Bismuth Eutectic Alloy and Properties, Materials Compatibility, Thermal-Hydraulics and Technologies
(
OECD/NEA
,
Paris
,
2015
), NEA. No. 7268.
3.
O.
Yeliseyeva
,
V.
Tsisar
, and
Z.
Zhou
,
J. Nucl. Mater.
442
,
434
(
2013
).
4.
M.
Roy
,
L.
Martinelli
,
K.
Ginestar
,
J.
Favergeon
, and
G.
Moulin
,
J. Nucl. Mater.
468
,
153
(
2016
).
5.
O. I.
Yeliseyva
,
V. P.
Tsisar
,
I.
Ivanova
, and
A. M.
Demidik
,
Powder Metall. Met. Ceram.
47
,
607
(
2008
).
6.
7.
8.
A.
Weisenburger
 et al,
J. Nucl. Mater.
415
,
260
(
2011
).
9.
G.
Muller
,
A.
Heinzel
,
J.
Konys
,
G.
Schumacher
,
A.
Weisenburger
,
F.
Zimmermann
,
V.
Engelko
,
A.
Rusanov
, and
V.
Markov
,
J. Nucl. Mater.
335
,
163
(
2004
).
10.
A. K.
Rivai
and
M.
Takahashi
,
J. Nucl. Mater.
398
,
146
(
2010
).
11.
G.
Müller
,
G.
Schumacher
, and
F.
Zimmermann
,
J. Nucl. Mater.
278
,
85
(
2000
).
12.
G.
Müller
,
A.
Heinzel
,
J.
Konys
,
G.
Schumacher
,
A.
Weisenburger
,
F.
Zimmermann
,
V.
Engelko
,
A.
Rusanov
, and
V.
Markov
,
J. Nucl. Mater.
301
,
40
(
2002
).
13.
A.
Heinzel
,
M.
Kondo
, and
M.
Takahashi
,
J. Nucl. Mater.
350
,
264
(
2006
).
14.
Y.
Kurata
,
M.
Futakawa
, and
S.
Saito
,
J. Nucl. Mater.
335
,
501
(
2004
).
15.
F.
Garcia Ferré
,
M.
Ormellese
,
F.
Di Fonzo
, and
M. G.
Beghi
,
Corros. Sci.
77
,
375
(
2013
).
16.
V.
Engelko
,
G.
Mueller
,
A.
Rusanov
,
V.
Markov
,
K.
Tkachenko
,
A.
Weisenburger
,
A.
Kashtanov
,
A.
Chikiryaka
, and
A.
Jianu
,
J. Nucl. Mater.
415
,
270
(
2011
).
17.
H.
Glasbrenner
and
F.
Groschel
,
J. Nucl. Mater.
356
,
213
(
2006
).
18.
T. C.
Chou
,
T. G.
Nieh
,
S. D.
McAdmams
, and
G. M.
Pharr
,
Scr. Metall. Mater.
25
,
2203
(
1991
).
19.
R.
Cremer
,
K.
Reichert
,
D.
Neuschitz
,
G.
Erkens
, and
T.
Leyendercher
,
Surf. Coat. Technol.
163
,
157
(
2003
).
20.
O.
Kyrylov
,
R.
Cremer
, and
D.
Neuschutz
,
Surf. Coat. Technol.
163
,
203
(
2003
).
21.
G.
Erkens
,
Surf. Coat. Technol.
201
,
4806
(
2007
).
22.
S. M.
Rossnagel
 et al,
Handbook of Plasma Processing Technology
(
Noyes Publication
,
NJ
,
1990
), p.
233
.
23.
M.
Ohring
,
Materials Science of Thin Films
(
Academic
,
San Diego, CA
,
1992
), p.
126
.
24.
M.
Schneider
,
W. D.
Sproul
,
A. A.
Voevodin
, and
A.
Matthews
,
J. Vac. Sci. Technol., A
15
,
1084
(
1997
).
25.
T.
Roth
,
K. H.
Kloos
, and
E.
Broszeit
,
Thin Solid Films
153
,
123
(
1987
).
26.
T.
Hubert
,
S.
Svoboda
, and
B.
Oertel
,
Surf. Coat. Technol.
201
,
487
(
2006
).
27.
K. S.
Sree Harsha
,
Principles of Physical Vapor Deposition of Thin Films
, 1st ed. (
Oxford
,
Elsevier
,
2006
).
28.
F.
Di Grabriele
,
S.
Amore
,
C.
Scaiola
,
E.
Arato
,
D.
Giuranno
, and
R.
Novakovic
,
Nucl. Eng. Des.
280
,
69
(
2014
).
29.
W.
Rasband
, “
Image J 1.48v
,” National Institute of Health, http://imagej.nih.gov/ij
30.
J. M.
Fildes
,
S. J.
Meyers
,
R.
Kilaparti
, and
E.
Schlepp
,
Wear
274
,
414
(
2012
).
31.
L.
Lutterotti
,
D.
Chateigner
,
S.
Ferrari
, and
J.
Ricote
,
Thin Solid Films
450
,
34
(
2004
).
32.
L.
Lutterotti
,
Nucl. Instrum. Methods B
268
,
334
(
2010
).
33.
R. A.
Young
,
The Rietveld Method
(
International Union of Crystallography, Oxford University
,
1993
).
34.
European standard UNI, EN 1071-3, “
Advanced technical ceramics—Methods of test for ceramic coatings—Part 3: Determination of adhesion and other mechanical failure modes by a scratch test
,” (
2005
).
35.
O.
Zywitzki
,
G.
Hoetzsch
,
F.
Fietzke
, and
K.
Goedicke
,
Surf. Coat. Technol.
82
,
169
(
1996
).
36.
G.
Liu
,
C.
Wang
,
F.
Yu
, and
J.
Tian
,
Oxid. Met.
81
,
383
(
2014
).
You do not currently have access to this content.