A customized atomic layer deposition (ALD) reactor was designed with components compatible with hydrogen sulfide (H2S) chemistry. H2S is used as a reactant for the ALD of metal sulfides. The use of H2S in an ALD reactor requires special attention to safety issues due to its highly toxic, flammable, and corrosive nature. The reactor was designed with respect to materials compatibility of all wetted components with H2S. A customized safety interlock system was developed to shut down the system in the event of toxic gas leakage, power outage, loss of building ventilation or compressed air pressure. ALD of lead sulfide (PbS) and zinc sulfide (ZnS) were demonstrated with no chemical contamination or detectable release of H2S.

1.
M.
Ritala
and
M.
Leskelä
,
Nanotechnology
10
,
19
(
1999
).
2.
J.
Elam
,
D.
Routkevitch
,
P. P.
Mardilovich
, and
S. M.
George
,
Chem. Mater.
15
,
3507
(
2003
).
3.
P. -C.
Su
,
C. -C.
Chao
,
J. H.
Shim
,
R.
Fasching
, and
F. B.
Prinz
,
Nano Lett.
8
,
2289
(
2008
).
4.
P.
Banerjee
,
I.
Perez
,
L.
Henn-Lecordier
,
S. B.
Lee
, and
G. W.
Rubloff
,
Nat. Nanotechnol.
4
,
292
(
2009
).
5.
A. B. F.
Martinson
,
J. W.
Elam
,
J. T.
Hupp
, and
M. J.
Pellin
,
Nano Lett.
7
,
2183
(
2007
).
6.
M.
Knez
,
A.
Kadri
,
C.
Wege
,
U.
Gösele
,
H.
Jeske
, and
K.
Nielsch
,
Nano Lett.
6
,
1172
(
2006
).
7.
X.
Zhang
,
J.
Zhao
,
A. V.
Whitney
,
J. W.
Elam
, and
R. P.
Van Duyne
,
J. Am. Chem. Soc.
128
,
10304
(
2006
).
8.
J. S.
King
,
C. W.
Neff
,
C. J.
Summers
,
W.
Park
,
S.
Blomquist
,
E.
Forsythe
, and
D.
Morton
,
Appl. Phys. Lett.
83
,
2566
(
2003
).
9.
E. B.
Yousfi
,
T.
Asikainen
,
V.
Pietu
,
P.
Cowache
,
M.
Powala
, and
D.
Lincot
,
Thin Solid Films
361–362
,
183
(
2000
).
10.
N.
Naghavi
,
R.
Henriquez
,
V.
Laptev
, and
D.
Lincot
,
Appl. Surf. Sci.
222
,
65
(
2004
).
11.
S.
Spiering
,
D.
Hariskos
,
S.
Schröder
, and
M.
Powalla
,
Thin Solid Films
480–481
,
195
(
2005
).
12.
L.
Reijnen
,
B.
Meester
,
A.
Goossens
, and
J.
Schoonman
,
Chem. Vap. Deposition
9
,
15
(
2003
).
13.
A. F.
Martinson
,
J. W.
Elam
, and
M. J.
Pellin
,
Appl. Phys. Lett.
94
,
123107
(
2009
).
14.
T.
Suntola
and
J.
Hyvärinen
,
Annu. Rev. Mater. Sci.
15
,
177
(
1985
).
15.
M.
Leskelä
and
M.
Ritala
,
J. Phys. IV
9
,
Pr8
(
1999
).
16.
G.
Stuyven
,
P.
De Visschere
,
A.
Hikavyy
, and
K.
Neyts
,
J. Cryst. Growth
234
,
690
(
2002
).
17.
M.
Leskelä
,
L.
Niinistö
,
P.
Niemela
,
E.
Nykänen
,
P.
Soininen
,
M.
Tiita
, and
J.
Vähäkangas
,
Vacuum
41
,
1457
(
1990
).
18.
E.
Nykänen
,
J.
Laine-Ylijoki
,
P.
Soininen
,
L.
Niinistö
,
M.
Leskelä
, and
G.
Hubert-Pfalzgraf
,
J. Mater. Chem.
4
,
1409
(
1994
).
19.
N. P.
Dasgupta
,
W.
Lee
, and
F. B.
Prinz
,
Chem. Mater.
21
,
3973
(
2009
).
20.
Hydrogen Sulfide; MSDS No. P-4611-G; Praxair Inc.: Danbury, CT, May,
2009
.
21.
R. J.
Reiffenstein
,
Annu. Rev. Pharmacol. Toxicol.
32
,
109
(
1992
).
22.
A. R.
Hirsch
and
G.
Zavala
,
Occup. Environ. Med.
56
,
284
(
1999
).
23.
Kirk-Othmer Encyclopedia of Chemical Technology
,
Sulfur Compounds: Hydrogen Sulfide
, 5th ed., edited by
A.
Seidel
(
Wiley-Interscience
,
Hoboken
,
2007
), Vol.
23
.
25.
Plastics Design Library Staff
,
Chemical Resistance of Plastics and Elastomers
, 4th ed. (
William Andrew Publishing/Plastics Design Library
,
Norwich
,
2008
).
26.
“Extended Cycle Test of Swagelok® ALD6 Series Diaphragm Valve Under Vacuum,” Swagelok Product Test Report, PTR-1691, April
2008
.
27.
B. H.
Chudnovski
,
Proceedings of the 48th IEEE Holm Conference on Electrical Contacts
,
2002
, p.
140
.
You do not currently have access to this content.