Variable liquid crystal pretilt angles of any value from 0 to 90° can be obtained by using a nanostructured alignment layer. This layer is robust and reliable. The pretilt angles obtained are stable against high storage and operating temperatures, and have strong anchoring energies.
REFERENCES
1.
T.
Uchida
, M.
Ohgawara
, and M.
Wada
, Jpn. J. Appl. Phys., Part 1
19
, 2127
(1980
).2.
R. W.
Filas
and J. S.
Patel
, Appl. Phys. Lett.
50
, 1426
(1987
).3.
M.
Schadt
, H.
Seiberle
, and A.
Schuster
, Nature (London)
381
, 221
(1996
).4.
M.
Nishikawa
, B.
Taheri
, and J. L.
West
, Proceedings of the Society for Information Display International Symposium
, 1998
, Vol. 29
, p. 131
.5.
F. S.
Yeung
, F. C.
Xie
, H. S.
Kwok
, J.
Wan
, O.
Tsui
, and P.
Sheng
, Proceedings of the Society for Information Display International Symposium
, 2005
, Vol. 36
, p. 1080
.6.
J. T.
Wan
, O. K.
Tsui
, H. S.
Kwok
, and P.
Sheng
, Phys. Rev. E
72
, 021711
(2005
).7.
V.
Chigrinov
, A.
Muravski
, H. S.
Kwok
, H.
Takada
, H.
Akiyama
, and H.
Takatsu
, Phys. Rev. E
68
, 061702
(2003
).8.
F. S.
Yeung
, A.
Muravski
, Y. W.
Li
, V.
Chigrinov
, and H. S.
Kwok
(unpublished).9.
F. S. Y.
Yeung
, Y. W.
Li
, and H. S.
Kwok
, Proceedings of the Society for Information Display International Symposium
, 2005
, Vol. 36
, p. 1770
.© 2006 American Institute of Physics.
2006
American Institute of Physics
You do not currently have access to this content.